Materjali keemiline koostis
| Hinne | element | C | Mn | P | S |
| ASTM A500 Gr.b | protsenti | 0,05 protsenti -0,23 protsenti | 0,3 protsenti -0,6 protsenti | 0,04 protsenti | 0,04 protsenti |
| Vastavalt standardile EN10027/1 | Vastavalt standardile EN10027/2 | C protsenti max (tavaline WT (mm) | Si protsent max | Mn protsenti max | P protsenti max | S protsenti max | N protsenti max | |
| ja IC 10 | Vähem kui 40 või sellega võrdne | |||||||
| S235JRH | 1.0039 | 0.17 | 0.20 | - | 1.40 | 0.045 | 0.045 | 0.009 |
| S275JOH | 1.0149 | 0.20 | 0.22 | - | 1.50 | 0.040 | 0.040 | 0.009 |
| S275J2H | 1.0138 | 0.20 | 0.22 | - | 1.50 | 0.035 | 0.035 | - |
| S355JOH | 1.0547 | 0.22 | 0.22 | 0.55 | 1.60 | 0.040 | 0.040 | 0.009 |
| S355J2H | 1.0576 | 0.22 | 0.22 | 0.55 | 1.60 | 0.035 | 0.035 | - |
Materjali mehaanilised omadused
| Hinne | Saagikuse tugevus | Tõmbetugevus | Pikendamine |
| A500.Gr.b | 46 ksi | 58 ksi | 23 protsenti |
| A513.GR.B | 72 ksi | 87 ksi | 10 protsenti |
| Norm | Saagikuse tugevus | Tõmbetugevus | Min.elogation | Min.protsent omadused | ||||||||
Vastavalt standardile EN10027/1 ja IC 10 | Vastavalt standardile EN10027/2 | Normaalne WTmm | Normaalne WTmm | Longit. | Rist | Testi temperatuuri aste | Keskmine minimaalne mõju väärtus | |||||
| Väiksem või võrdne 16 | >6 | >40 | <> | Väiksem või võrdne 3 Väiksem või võrdne 65 | Normaalne WTmm | |||||||
| Vähem kui 65 või sellega võrdne | Vähem kui 65 või sellega võrdne | Vähem kui 40 või sellega võrdne | >40 | >40 | Vähem kui 65 või sellega võrdne | |||||||
| Vähem kui 65 või sellega võrdne | Vähem kui 40 või sellega võrdne | |||||||||||
| S253JRH | 1.0039 | 235 | 225 | 215 | 360-510 | 340-470 | 26 | 25 | 24 | 23 | 20 | 27 |
| S275JOH | 1.0149 | 275 | 265 | 255 | 410-580 | 410-560 | 22 | 21 | 20 | 19 | 0 | 27 |
| S275J2H | 1.0138 | 275 | 265 | 255 | 430-560 | 410-560 | 22 | 21 | 20 | 19 | -20 | 27 |
| S355JOH | 1.0547 | 355 | 345 | 335 | 510-680 | 490-630 | 22 | 21 | 20 | 19 | 0 | 27 |
| S355J2H | 1.0576 | 355 | 345 | 335 | 510-680 | 490-630 | 22 | 21 | 20 | 19 | -20 | 27 |
Samaväärsed spetsifikatsioonid
ET 10210-1 | NF A 49501 NF A 35501 | DIN 17100 DIN 17123/4/5 | BS 4360 | UNI 7806 |
| S235JRH | E 24-2 | St 37.2 | – | Fe 360 B |
| S275JOH | E 28-3 | St 44.3 U | 43 C | Fe 430 C |
| S275J2H | E 28-4 | St 44.3 N | 43 D | Fe 430 D |
| S355JOH | E 36-3 | St 52.3 U | 50 C | Fe 510 C |
| S355J2H | E 36-4 | St 52.3 N | 50 D | Fe 510 D |
| S275NH | – | St E 285 N | – | – |
| S275NLH | – | TSt E 285 N | 43 EE | – |
| S355NH | E 355 R | St E 355 N | – | – |
| S355NLH | – | TSt E 355 N | 50 EE | – |
| S460NH | E 460 R | St E 460 N | – | – |
| S460NLH | – | TSt E 460 N | 55 EE | – |
– trükitäht "S" tähendab "TERAS KONSTRUKTSIOONIDEKS"
– järgmine arv tähendab miinimumi. seinapaksuse nõutav tootlikkus Vähem kui 16 mm või sellega võrdne
– "J2" tähendab löögitesti väärtust -20 kraadi C min. 27 džauli
– trükitäht "H" tähendab "ÕÕNE LÕIK".
Tootja: LEFIN STEEL
Tootmisvahemik: 20X20--1200X1200 20X30--1000X1500 paksus: 1.5-50mm Pikkus:1-25M
Tootmisvõimsus: 30000 tonni kuus
Tarneaeg: 20 päeva -- 30 päeva pärast esialgse LC kättesaamist
Contact: 008615122229899(whatsapp) ericli@lefinsteel.com







Kuum tags: astm a500 õõnesprofiilid, Hiina, tarnijad, tootjad, tehas, hind